Re: bar with high tension strength



oops, my name was somewhat screwed in the post before... now it's correct.

"gryf Deren" <[EMAIL PROTECTED]> schrieb im Newsbeitrag
news:[EMAIL PROTECTED]
> ceramics won't do it, not at 2500MPa
>
> I suggest using steel, the choices are limited at this very high tensile
> strength.
>
> Maraging steel will do it. I think material cost is not such a big issue
for
> this application, you won't need tons? Contact a specialty steel dealer,
> they can surely help you.
>
> "mango" <[EMAIL PROTECTED]> schrieb im Newsbeitrag
> news:[EMAIL PROTECTED]
> > Hi
> >
> > I need a 1.6 mm bar (metal or else) with more than 2500 mpa tension
> strength.
> >
> > And I have no idea where to start looking for it, any ideas?
>
>