Re: bar with high tension strength



ceramics won't do it, not at 2500MPa

I suggest using steel, the choices are limited at this very high tensile
strength.

Maraging steel will do it. I think material cost is not such a big issue for
this application, you won't need tons? Contact a specialty steel dealer,
they can surely help you.

"mango" <[EMAIL PROTECTED]> schrieb im Newsbeitrag
news:[EMAIL PROTECTED]
> Hi
>
> I need a 1.6 mm bar (metal or else) with more than 2500 mpa tension
strength.
>
> And I have no idea where to start looking for it, any ideas?