Re: Looking for oxydation protection of graphite



Look up ceraset (.com) - paint it on and pyrolize it. They (Kion Corporation)
have othersimilar chemicals. I've used ceraset on carbon-carbon.

Christine Gagnon wrote:

> I am looking for a paint, surface treatment or coating to prevent or delay
> oxydation of graphite in contact with both air and molten aluminum.