As far as I know there is no such metal readily availabele at this wire/bar diameter. "mango" <[EMAIL PROTECTED]> wrote in message news:[EMAIL PROTECTED] > Hi all > > I need a special metal bar with 1.6 mm thikness and >2500 mpa tension strength. > I even dont have a clue where to look for it? > Can any body help me out? > > Bubu