Interested in telling how you did it? I have a 230Amp AC buzzbox I wouldn't mind converting. Paul On Fri, 28 Nov 2003 14:17:09 -0500, billh wrote: > > "John D. Farr" <[EMAIL PROTECTED]> wrote in message > news:[EMAIL PROTECTED] >> [quoted text muted] > > I am not an expert welder but did convert an AC buzz box to DC for a bit of > fun and since DC seemed to be preferred or at least more popular than AC. I > found that using DC made it easier to get the arc started.