Dear DaveC: "DaveC" <[EMAIL PROTECTED]> wrote in message news:[EMAIL PROTECTED] > > > You might try "Sci.polymers" for more responces. > > Thanks, I will. > > > In order to get a better idea of the rigidity needed, what types of > > epoxy have you tried that were not acceptible? > > Devcon 5-minute epoxy was too soft (what I call too "resin-y"). Devcon is > what I have available at all the stores, locally. Some 3M stuff is available > at outrageous cost at the industrial supply house, but if that's what is > recommended, I can use that. Is there a reason why you do not use: - a "lossy" epoxy with a ground glass filler, or - cyanoacrylate (super glue)? Davdi A. Smith