Wumpus <[EMAIL PROTECTED]> wrote in news:QIydnaU5FJ9ru1OiRVn-
[EMAIL PROTECTED]:

> 
>> Are you sure you don't mean copper red? Tenmoku is black and tan
> 
> Oh, sorry, you're right. This was a glaze where the red was hard to get, 
> but when it didn't happen it was black. But the red was very deep and 
> beautiful.
> 
> 

If you mail me at

[EMAIL PROTECTED]

with your email address I will forward you a photo of a copper red reduced 
in a gas kiln and a copy of the recipe