The kiln insulation is adequate--you should always wait to crack the kiln open till below 500 degrees (or when paper ignites...). If you wait 15-20 hours, you won't even need to crack it open. I've fired hundreds of cone 10 electric kilns in northern winter conditions... The worst is leaving it too long to cool and unloading a bunch of ice cube pots... Brad Sondahl -- For original art, music, pottery, and literature, visit my homepage http://sondahl.com Pottery sales page http://sondahl.freeyellow.com My music site at mp3.com http://www.mp3.com/stations/sondahl To reply to me directly, don't forget to take out the "garbage" from my address.