reglazing



I glazed a pot at Cone 6, but am not happy with the matte finish.  I would
like to put a clear gloss over top and refire the pot.  However, I am having
a hard time getting the glaze to cover.  I heated the pot in my oven, but
that didn't really work.

Does anyone have any suggestions on how best to reglaze?