Re: Painting on glass - BIG problem!



"Mary" <[EMAIL PROTECTED]> wrote in message news:<[EMAIL PROTECTED]>...
> Spoke with a mayco representative and they are no longer making the glass
> paints.   I can tell you however that a company called crest molds is making
> a glass paint for kiln firing that I am having good results with.

I guess that explains why I can't find them. Just when I find
something that's low fire enough before glass moves. And lead/cadmium
free. Figures.
Those that Crest sells, the Satelite/Unique paints are very high fire
aren't they? Something around 1500 degrees to mature I think I read?