HI Michele >Tiffany style is usually referring to copper foil. It sounds like you are >using lead came??? anyway, try a) 000 brass wool after drying, wipe lightly >then brush the patina on with a soft brush. b) hit the solder with Windex >immediately after soldering (do not wash) Leave flux there, just Windex, >wipe with paper towel, apply patina. Wash wash wash with dawn or other >degreaser. it gets really bright copper after polishing. m > Thanks for the comments. No - I'm using copper foil, but after foiling the glass pieces are soldered together and a solder bead is added where the pieces join. The idea is to patinate the solder back to copper. I don't know Windex - what is that ? (I'm based in the UK - maybe it's a product that's not available over here..?) Thanks Adrian Suffolk UK